Products >> Best quality cellulose welding materials welding rod AWS E6011

Best quality cellulose welding materials welding rod AWS E6011

Build Your Online Product Catalogs?



Description
Product Name: Best quality cellulose welding materials welding rod AWS E6011
Supply Ability: 100000 Ton
Related proudcts
Specifications 2.0 mm 2.5 mm 3.2mm 4.0mm 5.0mm 5.5mm
Price Term: FOB
Port of loading: Xingang
Minimum Order 20 kg
Unit Price: $0.8-1.5/kg

E6011 welding electrode carbon steel welding rod China supplier

Introduction:
E6011 is a kind of electrode with low-hydrogen potassium type coating. AC/DC+. All-position welding. soft stable arc, good fluidity and removability of slag, smooth appearance . The deposited metal has excellent mechanical properties. Excellent crack-resistance and good low temperature i***ct toughness.
Uses:
Used for welding medium-carbon steel and low-alloy steel structures,such as 16Mn, 09Mn2Si and A, B, D and E steel for ships, and also used for welding on thick plates and hard-to-weld carbon steel structures.
Chemical Composition (%)
Chemical Composition
C
Mn
Si
S
P
Ni
Cr
Mo
V
Guarantee Value
¡Ü0.12
¡Ü1.60
¡Ü0.75
¡Ü0.035
¡Ü0.040
¡Ü0.30
¡Ü0.20
¡Ü0.30
¡Ü0.08
General Result
0.07
1.22
0.50
0.016
0.011
0.05
0.06
0.01
0.04

Mechanical Properties of Deposited Metal
Test Item
T.S (***)
Y.S (***)
EL. (%)
CVN(J)
Guarantee Value
¡Ý490
¡Ý400
¡Ý22
¡Ý47(-20℃)
General Result
560
450
32
80

Reference Current (DC)
Diameter
¦µ2.5
¦µ3.2
¦Õ4.0
¦Õ5.0
Amperage
55 ~ 85
90 ~ 140
140 ~ 190
190~250

Notes:
1. The electrode must be preheated at the temperature of 350℃ for 1 hour. Preheat the rod whenever it is used.
2. The impurities such as rust, oil stains and moisture must be cleared off of the work piece.
3. Short arc is required to perform welding. Narrow weld path is preferred.

Contact Us
Company: Shijiazhuang Wannuo Technology Co., Ltd
Contact: Ms. Coco Peng
Address: No.99 Haishan Street, Luquan District, Shijiazhuang City, Hebei Province, China.
Postcode: 050000
Tel: 86 153 54210353
Fax: 86 153 54210353
E-mail:         


Copyright© Shijiazhuang Wannuo Technology Co., Ltd All Rights Reserved.
Tel : 86 153 54210353 Fax : 86 153 54210353
Powered by 86exporter.com